Böhler Welding, submerged arc wire, creep-resistant CrMo steels

BÖHLER C 9 MV-UP SAW wire

EN ISO classificationS S CrMo91 FB
AWS classificationEB9
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Shipping in 24 hfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What BÖHLER C 9 MV-UP SAW wire is used for

BÖHLER C 9 MV-UP is a submerged arc (SAW) wire for welding creep-resistant CrMo steels. It is used on boilers, steam pipelines, refinery installations and parts working at elevated temperature.

The wire joins materials such as 1.4903 and ASTM A 335. It is used on boilers and pressure vessels under statutory inspection, and submerged arc welding gives a very high deposition rate on long, repeatable welds.

  • Classification EN ISO: S S CrMo91 FB
  • AWS classification: EB9
  • Shielding: flux matched to the wire, no shielding gas
  • Diameters: 2.5 / 3.0 mm

Do not interrupt welding and do not let the joint drop below the interpass temperature before the fill is finished. Keep an even flux layer over the arc, too thin a layer exposes the arc and too thick a one spoils the bead shape. Watch the wire stick-out and the position of the head against the weld centre line, under a flux you cannot see the pool and a mistake shows only after the slag is chipped off. Thinner diameters suit root runs, thicker ones suit filling.

Fits

For which materials and machines

Base materials
  • 1.4903
  • ASTM A 335
Process and machines

Submerged arc wire, works on any sound machine for this process: welders.